Correlation of microstructural and mechanical properties of K-doped tungsten fibers used as reinforcement of tungsten matrix for high temperature applications

Research output: Contribution to journalArticle

Standard

Correlation of microstructural and mechanical properties of K-doped tungsten fibers used as reinforcement of tungsten matrix for high temperature applications. / Terentyev, Dmitry; Van Renterghem, Wouter; Tanure, Leandro; Dubinko, Andrii; Riesch, Johan; Lebediev, S.; Khvan, Tymofii; Verbeken, Kim; Coenen, J.W.; Zhurkin, Evgeni E.

In: International Journal of Refractory Metals & Hard Materials, Vol. 79, 02.2019, p. 204-216.

Research output: Contribution to journalArticle

Harvard

Author

Terentyev, Dmitry ; Van Renterghem, Wouter ; Tanure, Leandro ; Dubinko, Andrii ; Riesch, Johan ; Lebediev, S. ; Khvan, Tymofii ; Verbeken, Kim ; Coenen, J.W. ; Zhurkin, Evgeni E. / Correlation of microstructural and mechanical properties of K-doped tungsten fibers used as reinforcement of tungsten matrix for high temperature applications. In: International Journal of Refractory Metals & Hard Materials. 2019 ; Vol. 79. pp. 204-216.

Bibtex - Download

@article{fa70cd785dec47d2bd0a2098ab45be86,
title = "Correlation of microstructural and mechanical properties of K-doped tungsten fibers used as reinforcement of tungsten matrix for high temperature applications",
abstract = "Reinforcement of tungsten by tungsten fibers (Wf) is considered an attractive option to mitigate the intrinsic brittleness of this material and to possibly extend the operational temperature window to ensure safe operation of the plasma facing component. By now, it has been demonstrated that tungsten fiber-reinforced tungsten composites (Wf/W) acquire pseudo ductility even at room temperature, and crack propagation is determined by the interaction of the fibers with the propagating crack. In view of strong temperature oscillations, expected during operation in the fusion plasma, the mechanical properties of tungsten fibers annealed at different temperatures (up to 2300 °C) were assessed, and the role of potassium (K) doping on the modification of the mechanical properties of as-annealed wires was studied. While K-doping was found to delay the brittleness induced by heat exposure at least up to 1600 °C, still a strong reduction of the fiber strength was observed in tests performed at elevated temperatures. In this work, we investigate the reasons for this effect by performing scanning electron microscopy coupled with electron backscatter diffraction measurements. The longitudinal and transversal cross-sections of W fibers were analyzed to deduce the morphology and size distribution of the grains. Consistent with the mechanical data, we found that annealing at 2100 °C resulted in the full recrystallization of the elongated grains, otherwise formed due to the extrusion fabrication process. Even at 1900 °C, the longitudinal cross-section still exhibits elongated grains. The transversal shape of the grains undergoes a change from needle-like fine structure to equiaxed grain shape upon annealing above 1600 °C. Few scans done for 2300 °C annealed wire revealed that the microstructure contains one or several grains with a dimension of 70–150 μm. The obtained results are discussed and analyzed in the frame of mechanistic model connecting microstructure with the mechanical response.",
keywords = "Tungsten, Fiber, Plasticity, Recrystallization, Potassium doped, Annealing, Composites",
author = "Dmitry Terentyev and {Van Renterghem}, Wouter and Leandro Tanure and Andrii Dubinko and Johan Riesch and S. Lebediev and Tymofii Khvan and Kim Verbeken and J.W. Coenen and Zhurkin, {Evgeni E.}",
note = "Score=10",
year = "2019",
month = "2",
doi = "10.1016/j.ijrmhm.2018.12.007",
language = "English",
volume = "79",
pages = "204--216",
journal = "International Journal of Refractory Metals & Hard Materials",
issn = "0263-4368",
publisher = "Elsevier",

}

RIS - Download

TY - JOUR

T1 - Correlation of microstructural and mechanical properties of K-doped tungsten fibers used as reinforcement of tungsten matrix for high temperature applications

AU - Terentyev, Dmitry

AU - Van Renterghem, Wouter

AU - Tanure, Leandro

AU - Dubinko, Andrii

AU - Riesch, Johan

AU - Lebediev, S.

AU - Khvan, Tymofii

AU - Verbeken, Kim

AU - Coenen, J.W.

AU - Zhurkin, Evgeni E.

N1 - Score=10

PY - 2019/2

Y1 - 2019/2

N2 - Reinforcement of tungsten by tungsten fibers (Wf) is considered an attractive option to mitigate the intrinsic brittleness of this material and to possibly extend the operational temperature window to ensure safe operation of the plasma facing component. By now, it has been demonstrated that tungsten fiber-reinforced tungsten composites (Wf/W) acquire pseudo ductility even at room temperature, and crack propagation is determined by the interaction of the fibers with the propagating crack. In view of strong temperature oscillations, expected during operation in the fusion plasma, the mechanical properties of tungsten fibers annealed at different temperatures (up to 2300 °C) were assessed, and the role of potassium (K) doping on the modification of the mechanical properties of as-annealed wires was studied. While K-doping was found to delay the brittleness induced by heat exposure at least up to 1600 °C, still a strong reduction of the fiber strength was observed in tests performed at elevated temperatures. In this work, we investigate the reasons for this effect by performing scanning electron microscopy coupled with electron backscatter diffraction measurements. The longitudinal and transversal cross-sections of W fibers were analyzed to deduce the morphology and size distribution of the grains. Consistent with the mechanical data, we found that annealing at 2100 °C resulted in the full recrystallization of the elongated grains, otherwise formed due to the extrusion fabrication process. Even at 1900 °C, the longitudinal cross-section still exhibits elongated grains. The transversal shape of the grains undergoes a change from needle-like fine structure to equiaxed grain shape upon annealing above 1600 °C. Few scans done for 2300 °C annealed wire revealed that the microstructure contains one or several grains with a dimension of 70–150 μm. The obtained results are discussed and analyzed in the frame of mechanistic model connecting microstructure with the mechanical response.

AB - Reinforcement of tungsten by tungsten fibers (Wf) is considered an attractive option to mitigate the intrinsic brittleness of this material and to possibly extend the operational temperature window to ensure safe operation of the plasma facing component. By now, it has been demonstrated that tungsten fiber-reinforced tungsten composites (Wf/W) acquire pseudo ductility even at room temperature, and crack propagation is determined by the interaction of the fibers with the propagating crack. In view of strong temperature oscillations, expected during operation in the fusion plasma, the mechanical properties of tungsten fibers annealed at different temperatures (up to 2300 °C) were assessed, and the role of potassium (K) doping on the modification of the mechanical properties of as-annealed wires was studied. While K-doping was found to delay the brittleness induced by heat exposure at least up to 1600 °C, still a strong reduction of the fiber strength was observed in tests performed at elevated temperatures. In this work, we investigate the reasons for this effect by performing scanning electron microscopy coupled with electron backscatter diffraction measurements. The longitudinal and transversal cross-sections of W fibers were analyzed to deduce the morphology and size distribution of the grains. Consistent with the mechanical data, we found that annealing at 2100 °C resulted in the full recrystallization of the elongated grains, otherwise formed due to the extrusion fabrication process. Even at 1900 °C, the longitudinal cross-section still exhibits elongated grains. The transversal shape of the grains undergoes a change from needle-like fine structure to equiaxed grain shape upon annealing above 1600 °C. Few scans done for 2300 °C annealed wire revealed that the microstructure contains one or several grains with a dimension of 70–150 μm. The obtained results are discussed and analyzed in the frame of mechanistic model connecting microstructure with the mechanical response.

KW - Tungsten

KW - Fiber

KW - Plasticity

KW - Recrystallization

KW - Potassium doped

KW - Annealing

KW - Composites

UR - https://ecm.sckcen.be/OTCS/llisapi.dll/overview/37612564

U2 - 10.1016/j.ijrmhm.2018.12.007

DO - 10.1016/j.ijrmhm.2018.12.007

M3 - Article

VL - 79

SP - 204

EP - 216

JO - International Journal of Refractory Metals & Hard Materials

JF - International Journal of Refractory Metals & Hard Materials

SN - 0263-4368

ER -

ID: 6743742